Location:Home > Products > Coating

Single Wavelength AR Coatings

图片12.png

Substrate Substrate: fused silica, BK7 

Surface Figure: <λ/10 @ 632.8nm 

Surface Quality: 40-20 

Chamfer: 0.5mm, 45° 

Coating Material: Electron beam deposited dielectric multi-layers 

Incident:0° 

Clear Aperture: > Central 85% of diameter

Wavelength (nm)

Resldual Refiectance

193

<0.5%

284

<0.5%

355

<0.2%

632.8

<0.2%

670

<0.2%

780

<0.2%

808

<0.2%

980

<0.2%

1030

<0.2%

1053

<0.2%

1064

<0.2%

1310

<0.15%

1550

<0.15%



Dual Wavelength AR Coatings

图片12_1.png

Substrate fused silica, BK7 

Surface Figure <λ/10 @ 632.8nm 

Surface Quality 40-20 

Chamfer 0.5mm, 45° 

Coating Material Electron beam deposited dielectric multi-layers 

Incident 0° 

Clear Aperture > Central 85% of diameter

Wavelength (nm)

Resldual Refiectance

166/532

0.5%/0.3%

351/1053  

0.5%/0.3%

373/745

0.5%/0.3%

532/1064

0.5%/0.3%

1064/1535

0.5%/0.3%

792/2060

0.5%/0.3%